ALLOY 400. NOTE THE EXCEPTIONALY CLEAN, HIGH ENERGY FLUID WELD. ZERO WELD DEFECTS. INSTEAD OF THE TYPICAL 25-30 IPM FROM THE TIG WELDER TIP TIG DELIVERED 300 IPM